Research

Engineering Sciences

Title :

Effect of silver & scandium addition on stress corrosion cracking resistance of aluminum alloy AA7050

Area of research :

Engineering Sciences

Focus area :

Directorate of Extramural Research & Intellectual Property Rights, ER & IPR

Principal Investigator :

Dr. K.T. Kashyap, Professor, Siddaganga Institute of Technology, Karnataka

Timeline Start Year :

2019

Timeline End Year :

2022

Details

Total Budget (INR):

71,14,000

Organizations involved